Volume discount: 5 pcs 2% · 10 pcs 3% · 25 pcs 5%The Floor Was Laid on Concrete That Looked Dry, but the Moisture Meter Had Said OtherwiseHow to check your thermocouple thermometer yourself without an ice bath or dry blockAir in the fridge responds in minutes, food in hours – so measure with a probe that behaves like the foodCarbon dioxide levels show whether ventilation is working, something temperature never revealsWhen the temperature is read in 0.4 seconds, checking becomes routine rather than an interruptionThe temperature was right at the check, but what happened at three in the morning?A clogged filter first shows up as a pressure drop, but only if you measure across itOne Drop Is Enough: How to Check Sugar Content and Cutting Fluid Concentration in SecondsHow to know your thermometer reads correctly: check your instruments yourself between -10 and 110 °CThe surface shows one temperature, the core another: why you need both IR and a penetration probeVolume discount: 5 pcs 2% · 10 pcs 3% · 25 pcs 5%The Floor Was Laid on Concrete That Looked Dry, but the Moisture Meter Had Said OtherwiseHow to check your thermocouple thermometer yourself without an ice bath or dry blockAir in the fridge responds in minutes, food in hours – so measure with a probe that behaves like the foodCarbon dioxide levels show whether ventilation is working, something temperature never revealsWhen the temperature is read in 0.4 seconds, checking becomes routine rather than an interruptionThe temperature was right at the check, but what happened at three in the morning?A clogged filter first shows up as a pressure drop, but only if you measure across itOne Drop Is Enough: How to Check Sugar Content and Cutting Fluid Concentration in SecondsHow to know your thermometer reads correctly: check your instruments yourself between -10 and 110 °CThe surface shows one temperature, the core another: why you need both IR and a penetration probe

The Floor Was Laid on Concrete That Looked Dry, but the Moisture Meter Had Said Otherwise

Published 28 November 2026 at 12:56

A parquet floor is laid on a concrete slab that felt dry and looked dry. A few months later the joints have lifted and a complaint is a fact. The same thing happens with plasterboard that is painted too early after water damage, or timber that is built in before it has stabilised. Moisture is rarely something you can judge by eye, and guessing wrong is expensive.

ETI moisture meter complete with probes and carrying case. Based on meter 7000. For moisture measurement in wood, plasterboard and concrete. With digital readout and LED scale for easy viewing. Replaceable pin probes

What’s included in the kit

This is ETI’s moisture meter kit based on meter 7000. It consists of the instrument itself, a general-purpose two-pin probe, a heavy-duty hammer probe, 50 universal pins and 10 spare pins for the hammer probe, a yellow silicone cover and an ABS carrying case. The meter has a digital readout with 0.1% resolution and an LED scale that lets you see the approximate level within a few seconds. It runs on three AAA batteries, gives about 350 hours of operation and comes with a two-year warranty.

Scales for different materials

Moisture in wood and moisture in concrete are not the same thing, which is why the meter has separate scales. Two wood scales cover 6 to 40% and 8 to 40% respectively, the plasterboard scale runs from 0.1 to 15% and the concrete scale from 0.5 to 12%. There is also a linear reference scale from 0 to 1000, which is useful for comparative measurements between different points in the same material. Accuracy is stated as ±1% moisture content.

How it is used in practice

Carpentry and the wood industry. Timber that is to be glued, surface-treated or built in should have the correct moisture content. With the pin probe you check deliveries on arrival and follow the drying process without having to saw the material open.

Plumbing and sanitary installations. After a leak or a bathroom renovation, you need to know where the wall is actually dry. Measure in a grid on plasterboard and wood behind the surface layer, note the values and measure again after drying. The hammer probe is used where the pins need to be driven into harder material.

Flooring and property maintenance. Before flooring, painting or wallpapering, check that the substrate is below the manufacturer’s limit value. Note that pin measurement in concrete is an indication. Where requirements are strict, for example for warranty-based measurement, it should be supplemented with a method prescribed by industry regulations.

Why it pays off

The cost of moisture damage is almost always many times higher than the price of the instrument: relaying floors, double work for painters and a worksite standing still while waiting for something to dry. The kit also includes more pins than you will need for a long time, and it comes in a case that withstands a workshop van and a building site. Documented readings before each stage of work also let you show that the substrate was approved when the work was carried out.

If you want to see all the specifications and what can be added as accessories, you will find them on the product page.